PEER-REVIEWED PUBLICATION

2026

A multifunctional graphene-integrated double-network nanocomposite hydrogel for dual strain-temperature wearable sensing

A tensile test divider icon

Romih A, Abdul Samad Y, Kim JK, Schiffer A

Advanced Composites and Hybrid Materials

Khalifa University of Science and Technology, Research and Innovation Center for Graphene and 2D Materials, Advanced Research and Innovation Center, University of New South Wales

RESEARCH SUMMARY
This study developed a multifunctional conductive double-network hydrogel combining chitosan, modified polyethylene glycol, and graphene nanoplatelets for wearable strain and temperature sensing. The hydrogel architecture combined a relatively rigid chitosan network with a flexible mPEG network, while graphene created conductive pathways and ethylene glycol improved resistance to dehydration. Graphene concentration strongly influenced mechanical and electrical performance. Low graphene contents of 0.05-0.10 wt% produced tensile strengths of approximately 1.50-1.85 MPa and fracture strains of 400-460%, while the optimized 0.15 wt% graphene formulation reached a tensile strength of 2.72 MPa with approximately 350% stretchability. Increasing graphene beyond this level reduced performance because of nanoparticle aggregation. Compression testing to 90% strain similarly demonstrated reinforcement with graphene addition. The optimized hydrogel showed stable mechanical behaviour during 500 tensile and compressive cycles at 50% strain, with little permanent deformation, decreasing energy dissipation over early cycles, and recovery increasing from approximately 83.5% to 90%. The material also exhibited intrinsic adhesion to metal, human skin, plastic, glass, and rubber, with corresponding adhesion energies of 189.6 ± 12.5, 115.6 ± 5.2, 102.4 ± 5.4, 64.4 ± 3.2, and 48.8 ± 4.6 J/m². Graphene increased electrical conductivity to 2.75 S/m at 0.15 wt%, and the optimized sensor achieved a gauge factor of 4.0 from 0-130% strain and an apparent average gauge factor of 13.8 from 130-350% strain. The hydrogel also exhibited a strong negative thermoresistive response, with a temperature coefficient of resistance of -5.62% °C⁻¹ between 28 and 40 °C. A dual-geometry sensing strategy using straight and winding hydrogel elements successfully separated strain and temperature signals, allowing reconstruction of both variables with low error. Ethylene glycol substantially improved seven-day ambient stability, preserving approximately 89% of initial mass and 79% of initial gauge factor. On-body tests demonstrated repeatable detection of wrist, finger, ankle, and elbow motion as well as fever-range temperature changes. Overall, the study establishes a mechanically robust, adhesive, dehydration-resistant graphene hydrogel capable of simultaneous strain and temperature monitoring for wearable healthcare and electronic-skin applications.
CellScale hexagons, without text

CELLSCALE INSTRUMENT USED

UniVert

A CellScale UniVert equipped with a 10 N load cell was used extensively for mechanical, electromechanical, adhesive, and temperature-response characterization of the chitosan/mPEG/graphene double-network hydrogels. For tensile testing, rectangular specimens measuring 20 × 5 × 2 mm with a 16 mm initial gauge length were stretched at 25 mm/min. Graphene loadings between 0 and 0.20 wt% were compared, and the UniVert measurements showed that the 0.15 wt% graphene formulation provided the best balance of strength and extensibility, reaching approximately 2.72 MPa tensile strength and 350% fracture strain. Compression tests were performed on 25 × 25 × 15 mm hydrogel specimens at 5 mm/min to strains as high as 90%, demonstrating increasing compressive strength with graphene reinforcement. The UniVert was also used for cyclic tensile and compressive testing of the optimized 0.15 wt% graphene hydrogel at 50% strain for 500 cycles. The material retained nearly overlapping loading-unloading behaviour with no obvious permanent deformation or structural damage, while tensile recovery increased from approximately 83.5% initially to about 90%. For electromechanical characterization, UniVert deformation was synchronized with resistance measurements from a digital multimeter, allowing calculation of strain sensitivity, cyclic signal stability, and gauge factor. The optimized formulation produced a gauge factor of 4.0 over 0-130% strain and approximately 13.8 over 130-350% strain. The UniVert was additionally used for standard 180° peel testing of the hydrogel on metal, human skin, plastic, glass, and rubber, quantifying plateau force, peel strength, and adhesion energy. Finally, the temperature-control module integrated with the UniVert was used to expose the sensor to controlled temperatures while electrical resistance was recorded. This enabled measurement of a -5.62% °C⁻¹ temperature coefficient of resistance from 28-40 °C and evaluation of fever-range sensing between approximately 36.5 and 37.8 °C. Together, these UniVert experiments established the hydrogel’s tensile strength, compressive resilience, cyclic durability, adhesion performance, electromechanical sensitivity, and temperature-sensing response.
AUTHORS

Amaal Romih, Yarjan Abdul Samad, Jang-Kyo Kim, Andreas Schiffer.

PUBLICATION DETAILS
JOURNAL

Advanced Composites and Hybrid Materials

YEAR

2026

INSTITUTIONS

Khalifa University of Science and Technology, Research and Innovation Center for Graphene and 2D Materials, Advanced Research and Innovation Center, University of New South Wales

COUNTRIES

Australia, United Arab Emirates

INSTRUMENT USED

UniVert

TESTING METHODS

Adhesion TestingCompression TestingFatigue TestingTensile Testing

RESEARCH APPLICATIONS

Adhesives and Sealants TestingHydrogel Mechanical TestingMaterial Fatigue and DurabilityStimuli Responsive Hydrogels CharacterizationWearable Bioelectronics

Related Publications:

Instrument Used:
Year:
Testing Method:
Research Application:
Country:

Contact Sales

Product of Interest:
CellScale hexagon shapes